| Appearance | | Light yellow, no obvious extraneous matter. | | | | | | | Visual Inspection |
| Density, g/cm3 | | 1.00~ 1.06 | 1.03~ 1.13 | 1.08~ 1.18 | 1.10~ 1.20 | 1.14~ 1.24 | 1.17~ 1.27 | 1.20~ 1.30 | ASTM D792 |
| Curing | Hardness, Shore A | 23±3 | 30±3 | 40±3 | 50±3 | 60±3 | 70±3 | 80±3 | ASTM D2240 |
| Tensile Strength, MPa ≥ | 5.0 | 5.5 | 6.5 | 8.0 | | 7.5 | 6.5 | ASTM D412 |
| Elongation at Break, % ≥ | 650 | 550 | 450 | 380 | 320 | 220 | 180 | |
| Tension Set, % ≤ | 8 | 7 | | 8 | | | 7 | |
| Tear Strength, Die C kN/m ≥ | 10 | 15 | 18 | 20 | | | 18 | ASTM D624 |
| Post-curing | Hardness, Shore A | 24±3 | 31±3 | 41±3 | 53±3 | 63±3 | 72±3 | 83±3 | ASTM D2240 |
| Tensile Strength, MPa ≥ | 4.5 | 6.0 | 7.0 | 7.5 | | | 7.0 | ASTM D412 |
| Elongation at Break, % ≥ | 600 | | 320 | 300 | 260 | 180 | 150 | |
| Tear Strength, Die C kN/m ≥ | 8 | 14 | 16 | 18 | | 20 | 16 | ASTM D624 |
| Compression Set, 180℃*22h ≤ | | 45 | 35 | 30 | | 25 | | | ASTM D395 |
| Property variation percent during aging (250℃*72h) | Hardness, Shore A | -5 | -3 | | | | 4 | 5 | / |
| Tensile Strength, % | -60 | -35 | | -30 | | | -15 | / |
| Elongation at Break, % | -40 | -20 | | -15 | -20 | -30 | -15 | / |